Janus银纳米层增强聚酰亚胺双层隔膜调控锂成核实现无枝晶锂金属电池
Janus Ag Nanoskin‐Armored Polyimide Bilayer Separator Enables Efficient Li‐Nucleation Regulation for Dendrite‐Free Lithium Metal Battery
研发导读
研究团队在聚酰亚胺纳米纤维表面原位生长银纳米颗粒并复合高强度聚酰亚胺膜,制备出Janus Ag@PI/PI双层隔膜,利用银纳米层作为亲锂三维宿主诱导锂顺序成核。
研发阅读价值
该隔膜以银纳米层诱导锂顺序沉积,其成核过电位与Li||NCM523倍率数据可供界面调控方案比较。